MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

KiON CLEAR Ambient Cure, Polysilizane Clear Coat  (discontinued **)
Categories: Fluid; Polymer; Thermoset

Material Notes: KiON Clear is a crystal clear, ready-to-use Polysilazane clear coat. When applied, KiON Clear cures at ambient temperature by a moisture induced crosslinking mechanism. KiON Clear can easily be applied by spraying, dipping, or brush coating. KiON Clear can be used as an oxidation- or corrosion-resistant clear finish for metals, plastics, glass and other substrate materials. An average dry time of approximately 1 hour is typically achieved, depending upon temperature and humidity. KiON Clear provides a clear, protective coating for both ferrous and non-ferrous metals and alloys, ceramics, glass, etc. In addition, KiON Clear has excellent “weatherability”, UV resistance, hardness and abrasion resistance.

Applications

Clear, protective coatings for both ferrous and non-ferrous metals and alloys, clear automotive finishes, thermally durable coatings, and industrial, infrastructure and marine coatings.

Information provided by KiON Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.904 g/cc0.0327 lb/in³Liquid
Volatile Organic Compounds (VOC) Content 659 g/l659 g/l
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 26.0 °C>= 78.8 °F
 
Optical PropertiesMetricEnglishComments
Gloss 90 %90 %at 60 degrees
 
Descriptive Properties
%Resin23.7 wt% solids
Adhesion ASTM D 335990-100% on chromated aluminum
AppearanceClear, colorless
Chemical ResistanceMEK, Acetone, Brake Fluid, and most organic solvents
Pencil Hardness ASTM D 33636H on chrome treated aluminum
UV StabilityExcellent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKION08 / 48724

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.