A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical and thermal electrical conductivity are required. Forms: Information provided by Cadi Company. |
ASTM B441, ASTM B534, UNS C17510 |