MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

East Coast Precision Manufacturing
East Coast Precision Manufacturing - Ertalyte® Machining

(Viewing data as-entered. Click here to return)
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/cc
Mooney Viscosity 30 - 60
@Temperature 100 °C
ML(1+4)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 61press cure 11 min./160ºC
Tensile Strength 3390 psipress cure 11 min./160ºC
Elongation at Break 700 %press cure 11 min./160ºC
100% Modulus 0.160 ksi
@Strain 100 %
press cure 11 min./160ºC
200% Modulus 0.218 ksi
@Strain 200 %
press cure 11 min./160ºC
300% Modulus 0.334 ksi
@Strain 300 %
press cure 11 min./160ºC
Tear Strength 29.1 kN/mDie C, press cure 11 min./160ºC
 
Descriptive Properties
AppearancePale to yellow sheets or bales
Formulation as Tested0.3Stearic Acid
 1Struktol WB222
 100Millathane 76
 2TP-95 (DBEEA)
 25Ultrasil VN3
 4DiCup 40C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 92 E 5670 FCM Ester-Based TPU-For Food Contact
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact
Huntsman IROGRAN® A 85 P 4394 FCM Ether-Based TPU-For Food Contact
Overview of materials for Silicone Polyurethane, Ether Based
TSE Industries Millathane® 55 Millable Polyether Polyurethane Rubber, Typical 83A Compound

PMILL008 / 87052

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.