MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ ELCRIN™ WF006LiQ Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP ELCRIN WF006LiQ, utilizing ELCRIN iQ upcycling technology, is a 30% glass filled iQ PBT grade based on food contact compliant ingredients. Added features include PCR content, excellent strength, stiffness and dimensional stability. Potential applications may be water treatment pump, sanitation for kitchen/bath. This grade contains minimum 37% PCR weight content. Under test for Potable Water Approval : ACS,KTW, WRAS, W270, NSF.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,High Strength,Good dimensional stability,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccASTM D792
Density 1.54 g/cc0.0556 lb/in³ISO 1183
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.100 %0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.090 %0.090 %ISO 62-1
Viscosity 38 cP
@Load 5.00 kg,
Temperature 250 °C
38 cP
@Load 11.0 lb,
Temperature 482 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
0.0080 - 0.010 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 52 g/10 min
@Load 5.00 kg,
Temperature 250 °C
52 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 114 MPa16500 psi5 mm/min; ASTM D638
 139 MPa20200 psi5 mm/min; ISO 527
Tensile Strength, Yield 114 MPa16500 psi5 mm/min; ASTM D638
 139 MPa20200 psi5 mm/min; ISO 527
Elongation at Break 1.6 %1.6 %5 mm/min; ISO 527
 2.2 %2.2 %5 mm/min; ASTM D638
Elongation at Yield 1.6 %1.6 %5 mm/min; ISO 527
 2.2 %2.2 %5 mm/min; ASTM D638
Tensile Modulus 10.7 GPa1550 ksi1 mm/min; ISO 527
 11.8 GPa1710 ksi5 mm/min; ASTM D638
Flexural Strength 189 MPa27400 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 210 MPa30500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 210 MPa30500 psiyield, 2 mm/min; ISO 178
Flexural Modulus 9.10 GPa1320 ksi1.3 mm/min, 50 mm span; ASTM D790
 9.10 GPa1320 ksi2 mm/min; ISO 178
Izod Impact Notched 82.0 J60.5 ft-lbASTM D256
 83.0 J
@Temperature -30.0 °C
61.2 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 7.70 J/cm14.4 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 7.00 J5.16 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Dielectric Strength 23.0 kV/mm
@Thickness 3.20 mm
584 kV/in
@Thickness 0.126 in
in air; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  89.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 89.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test 200 °C392 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 217 °C423 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi)  203 °C
@Thickness 3.20 mm
397 °F
@Thickness 0.126 in
unannealed; ASTM D648
 207 °C
@Thickness 6.40 mm
405 °F
@Thickness 0.252 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 265 °C473 - 509 °F
Zone 2 245 - 255 °C473 - 491 °F
Zone 3 250 - 265 °C482 - 509 °F
Melt Temperature 250 - 265 °C482 - 509 °FInjection Molding
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 120 hour120 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00250 - 0.00380 cm0.000984 - 0.00150 in
Screw Speed 50 - 80 rpm50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80618 / 288565

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.