MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes:

Butene Copolymer

Features:

  • Excellent processability, cold temperature impact resistance and ESCR properties
  • Outstanding flexibility and warpage resistance
  • Good organoleptic properties and natural color
  • High surface gloss

Additives:

  • Processing antioxidant

Applications:

  • Thin wall lids for frozen food packaging (ice cream, whipped dairy)
  • Caps and closures, tamper evident, dairy applications
  • Compounding

United States: SCLAIR 2114 resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.1a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking.

Data provided by the manufacturer.

Key Words: Linear Low Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccASTM D792
ESCR 100% Igepal® <= 10 hourF50, Condition A, ASTM D1693
Melt Flow 52 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 36.0 cmNOVA Snake Flow Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ASTM D2240
Tensile Strength, Yield 10.0 MPa50 mm/min; ASTM D638
 12.0 MPa500 mm/min; ASTM D638
Elongation at Break 25 %500 mm/min; ASTM D638
 100 %50 mm/min; ASTM D638
Flexural Modulus 0.345 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 87.0 °CASTM D1525
Brittleness Temperature <= -70.0 °CASTM D696
 
Processing PropertiesOriginal ValueComments
Melt Temperature 170 - 215 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Novapol® PF-0118-B Butene LLDPE Film Resin
NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin
NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin
NOVA Chemicals Novapol® GM-1224-A Butene LLDPE Masterbatch Resin

PEHN1G / 35565

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.