MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT CHT-BeauSil™ WAX 069 Silicone wax
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Silicone waxes are more than an emollient in Personal Care. Silicone waxes are alkyl modified polydimethyl siloxanes that act different than classic silicone fluids in formulations. Outstanding performance is created by the alkyl modification which result in unique physical and chemical properties.

Key Features

  • Water repellency
  • Emollient, Softness and Smoothness, Reduces tackiness
  • Enhances spreading and solubilizing of natural lipids
  • Gives texture / structure
Key Applications
  • Skin Care
  • Color Cosmetic
  • Sun Care
Application: CHT-BeauSil™ WAX 069 improves the smoothness, detackification, lubricity gloss, emolliency and water repellency. It provides a higher spreadability, non-sticky feel and moisturizing benefits when it melts on contact with the skin. CHT-BeauSil™ WAX 069 improves the skin adhesion of decorative cosmetics and pigment dispersions. CHT-BeauSil™ WAX 069 avoids the syneresis in pigmented products (lipstick).

Addition Rates:
Dosage – 1: 0.5 – 5.0% in decorative and skin care preparations
Dosage – 2: 1.0 - 3.0% in sun care products

INCI Name: Stearyl dimethicone

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.00 %
Storage Temperature 4.00 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 30.0 - 32.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceColorless to slightly yellow wax
IonicityNon-ionic
MIT FreeYes
Ultralow cyclic contentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL367 / 314850

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.