MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Concrete Form Oil VOC
Categories: Fluid; Lubricant

Material Notes: Texaco Concrete Form Oil VOC delivers value through:
  • Clean separation from forms — imparts an excellent surface finish to concrete.
  • Minimal build-up on forms — providing longer form life
  • Rust protection to metal forms — provides protection during application and during short storage.
  • Low Volatile Organic Content — designed for use in those geographical regions with special requirements for VOC.

Texaco Concrete Form Oil VOC is a clear, light pale, non-staining premixed product containing mineral oil, a special mold release agent, and a light distillate which facilitates applications. It has a low viscosity and low pour point which allows for easy application year round. It possesses excellent mold release properties which results in attractive concrete surfaces without blowholes, chips or other blemishes.

Texaco Concrete Form Oil VOC is designed to keep forms clean, providing longer form life. It also provides excellent rust protection on steel forms during application and short storage. After demolding with Texaco Concrete Form Oil VOC, concrete surfaces are generally suitable for painting, epoxy and/or coating operations.

Texaco Concrete Form Oil VOC is specially formulated to meet local requirements for volatile organic compounds (VOC) and still provide the excellent performance of a concrete form oil.

Texaco Concrete Form Oil VOC is designed to provide clean and easy separation of concrete from wood, metal and other forms. The special mold release agents contained in this product reacts chemically with the alkali in the concrete to form an interfacial film which promotes separation from the form and imparts a smooth texture or satin finish to the concrete. It is designed to minimize sticking of the concrete to the form which results in excellent surface finishes.

Texaco Concrete Form Oil VOC is suitable for use on all types of forms, including steel, aluminum, hardwood, plywood, and epoxy-coated forms. It is suitable for use in indoor and outdoor conditions. It meets the South Coast Air Quality Management Districts Rule 1113-1 requirement for Volatile Organic Content.

Texaco Concrete Form Oil VOC may be brushed on or sprayed using conventional Cocrete Form Oil spraying equipment. For best results, it should be applied to only clean and dry surfaces as an ultra thin film. Pooling of the mold oil on forms should be avoided. It provides typical coverages of 800-1600 sq ft/gal on wood molds and 1600-3200 sq ft/gal on metal surfaces. Typical spraying pressures of 35-60 psi may be used to apply Texaco Concrete Form Oil VOC.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221518; MSDS Number: 11438

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 36.3 °
Viscosity Measurement 108Viscosity Index
Saybolt Viscosity at 100°F 52 SUS
Saybolt Viscosity at 210°F 34 SUS
Kinematic Viscosity at 40°C (104°F) 7.5 cSt
Kinematic Viscosity at 100°C (212°F) 2.2 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -18.0 °C
Flash Point 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Concrete, foamed blast furnace slag aggregate
Concrete, Lightweight
Autoclaved aerated concrete, 0.800 g/cc density
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete
Mitsubishi Chemical Advanced Materials Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite

WTEXA051 / 76930

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.