Hostacom EKG 2090T BLACK is a 40% glass fiber reinforced PP (coupled). It combines excellent stiffness properties with good dimensional stability and low creep under load at elevated temperatures. The product is available as a customized color matched, pellet form. This grade is delivered in black color version. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts Market: Automotive Processing Method: Injection Molding Information provided by LyondellBasell. |