MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Von Roll Damisol 3500 LoV Epoxy for Vacuum Pressure Impregnation
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key features of this grade: Very low organic emission epoxy resin. Excellent stability and low viscosity for easy impregnation. VOC-free.

Vacuum pressure impregnation (VPI) is mainly used when the penetration and filling factor of the resin need to be improved versus other processing options.

Vacuum pressure impregnation (VPI) is mainly used when the penetration and filling factor of the resin need to be improved versus other processing options.

Information provided by Von Roll.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 0.00 g/lVOC Free
Viscosity 600 cP
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °CUL 1446 TP rating MW 35
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 °CCuring Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVONR9990 / 249280

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.