MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chambroad Petrochemicals JTG F40, I-D Polymer Modified Asphalt
Categories: Other Engineering Material

Material Notes: Polymer Modified Asphalt: The modified asphalt adopts the straight-run modified special materials of our own refinery to meet customers’ customized indicators and performance through deep processing. The product features excellent stability, good high and low temperature performance, remarkable anti-aging and anti-fatigue performances and is widely used in expressways and Tibet border roads for border defense. Interms of the advance certificate, high-performance SBS modified asphalt and SBR modified asphalt have reached the international advanced level and the international leading level respectively.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity <= 3000 cSt
@Temperature 135 °C
T 0625/T 0619
 
Mechanical PropertiesOriginal ValueComments
Penetration 40 - 60
@Load 0.100 kg,
Time 5.00 sec
[0.1mm]; T 0604
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 230 °CT 0611
Ring & Ball Softening Point >= 60.0 °CT 0606
 
Descriptive Properties
Ductility>20 cm5?,5cm/min, T 0605
Elastic recovery>75%T 0662
Solubility>99%T 0607

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHAMB090 / 318632

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.