MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Ethomeen O/12 Oleyl amine ethoxylate
Categories: Other Engineering Material

Material Notes: Ethomeen O/12 is a tertiary amine ethoxylate, based on a primary oleyl amine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.904 g/cc0.0327 lb/in³
pH 11 - 1211 - 12
Viscosity 141 cP141 cPLV-2 spindle; 100 rpm
Vapor Pressure  0.000130 bar
@Temperature 20.0 °C
0.0975 torr
@Temperature 68.0 °F
 0.00390 bar
@Temperature 200 °C
2.93 torr
@Temperature 392 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 300 °C
@Pressure 0.101325 MPa
>= 572 °F
@Pressure 14.6921 psi
Initial
Pour Point -5.00 °C23.0 °F
Flash Point >= 200 °C>= 392 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 8.00.00 - 8.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %
 
Descriptive Properties
Amine number155-164 mg KOH/g
AppearanceLiquid
Clear point-5 °C
Cloud point45°C5 g in 25ml of 25/75% butyldiglycol/water
Content= 3 %Primary + Secondary Amine
 = 96 %Tertiary Amine
Equivalent mass343-363
HLB9.9Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY527 / 286050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.