MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Ecoterra® ISO Grade 100 Rock Drill Fluid
Categories: Fluid; Lubricant

Material Notes: Ecoterra Rock Drill Fluid is a high-quality, adhesive, extreme pressure (EP) lubricant specially developed for the lubrication of percussion rock drills used in surface and underground mining operations. It also is recommended for other air-powered tools such as jackhammers, pavement breakers and drifters. It is formulated with an ashless, chlorine-free additive package for reduced environmental impact. Ecoterra Rock Drill Fluid is specially formulated with select non-chlorinated additives to provide excellent protection for pneumatic percussion tools. It has high load-carrying capacity to protect against wear and seizure of sliding metal surfaces under heavy or shock-load conditions. It has good adhesiveness to metal surfaces in the presence of moisture, and contains inhibitors to protect against rust and corrosion. It has good oxidation resistance and thermal stability at high temperatures for long service life. The non-chlorinated additive package helps reduce environmental impact in case of leaks or stray mist, and facilitates waste oil disposal.

Applications:

  • Pneumatic equipment such as drifters, jackhammers, pavement breakers, rock drills and stoppers
Features/Benefit:
  • Non-chlorinated additive package for reduced environmental impact
  • Excellent extreme-pressure properties
  • Protects against wear and seizure
  • Good adhesiveness to metal surfaces in the presence of moisture
  • Good oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Low odor
  • Low fogging tendency
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.879 g/cc
Density 7.32 lb/gal
Viscosity Measurement 105Index
Saybolt Viscosity at 100°F 520 SUS
Saybolt Viscosity at 210°F 66.5 SUS
Kinematic Viscosity at 40°C (104°F) 100 cSt
Kinematic Viscosity at 100°C (212°F) 11.7 cSt
ASTM Color 3.5ASTM D1500
 
Mechanical PropertiesOriginal ValueComments
Timken Test 75.0 lbOK Load; ASTM D2782
 
Thermal PropertiesOriginal ValueComments
Pour Point -36.0 °C
Flash Point 208 °CCOC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5171 / 198424

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.