MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones KE-5551U High Strength Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: ShinEtsu KE5551 U is a nominal 50 Durometer base which offers high tensile and tear strengths. Its excellent processing characteristics make it suitable for molding, extrusion and calendaring

Product Features:

  • Minimum tear strength 168 ppi.
  • Translucent.
Typical Applications:
  • Gaskets.
  • Diaphragms.
  • Hose Stock.

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccDCBP Cure
 1.17 g/ccDBPH Cure
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50DCBP Cure
 50DBPH Cure
Tensile Strength at Break 1550 psiDBPH Cure
 1620 psiDCBP Cure
Elongation at Break 890 %DCBP Cure
 900 %DBPH Cure
Tear Strength 207 pliDie B; DCBP Cure
 218 pliDie B; DBPH Cure
Compression Set 46 %
@Temperature 177 °C,
Time 79200 sec
DCBP Cure
 
Descriptive Properties
Cure AgentDBPH
 DCBP
Cure TypePress Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-5560U Low Temperature Silicone Elastomer
Shin-Etsu Silicones KE-3421 Silicone, RTV Conformal Coating
Shin-Etsu Silicones KE-3475TUV Silicone, RTV Conformal Coating
Shin-Etsu Silicones KE-347T Silicone, RTV Coating
Shin-Etsu Silicones KE-441 Silicone, RTV

PSHIN227 / 177738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.