Compound 4705 is a 70 durometer black colored general purpose Neoprene elastomer. It exhibits good resistance to heat and compression set and it will remain non brittle at low temperatures. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 BC 715 A14 B14 C12 EO14 EO34 F17; 5 BC 715 A14 B14 C12 EO14 EO34 F19; 6 BC 715 A14 B14 C12 EO14 EO34 F17; 2 BE 715 A14 B14 EO14 EO34 F17; 3 BE 715 A14 B14 EO14 EO34 F19 AMS 3209 MIL-R-6855 Class 2a & 2b Grade 70 Information provided by Pressure Seals Inc. |