MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Esenttia 25C35-EC Impact Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Characteristics: Controlled rheology polypropylene homopolymer, medium molecular weight distribution, with high fluidity, with special additives for use on thin coatings at high line speeds to obtain excellent uniformity and adhesion, low neck-in, and thinning (draw-drown) and good properties.

Recommended for: Extrusion coating of raffia, paper and other substrates, aluminum and paper laminating.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238B
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.96 MPa4200 psi50 mm/min; ASTM D638
Elongation at Yield 9.5 %9.5 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1172.1 MPa170000 psi1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 0.395 J/cm0.740 ft-lb/inASTM D256-A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carmel Olefins CARMELCOAT™ MT 34 EC Specialty Polypropylene for Extrusion Coating
IRPC Polimaxx Polene 3375RM Polypropylene Random Copolymer
PolyMirae Moplen HP310R Extrusion Coating and Lamination Grade Polypropylene
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer
Reliance Industries Repol B250EG Polypropylene

PESEN051 / 184623

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.