MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Devcon® Floor Grip™ Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: 2-component, heavy-duty epoxy compound containing silicon carbide granules for anti-skid protection. Uses: Ideal anti-skid coating used in walkways; ramps; loading docks, and stairs. Features: Applies at temperatures as low as 40°F Reduces slipping accidents Adheres to concrete, wood, steel, brick, aluminum, and wet surfaces Bonds to damp surfaces Non-corrosive hardener.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity 2000 cP2000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 48.9 °C120 °FTemperature Resistance - Wet
 121 °C250 °FTemperature Resistance - Dry
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 32.2 °C40.0 - 90.0 °FApplication Temperature
Cure Time  480 min
@Temperature 24.0 °C
8.00 hour
@Temperature 75.2 °F
Foot Traffic
 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
Full service
 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
Functional cure
Pot Life 50.0 min
@Temperature 23.9 °C
50.0 min
@Temperature 75.0 °F
 
Descriptive Properties
Chemical/Solvent ResistanceAmmonia: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Chlorinated Solvent: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Kerosene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: very good30 day immersion at 75°F. Sample cured 7 days at RT
ColorBlackCured
Coverage80 ft²Cured. @ 16 mils
Mix Ratio by volume2.2:1
Mix Ratio by weight2.8:1
Recoat Time8 to 10 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9210 / 239719

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.