MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Advanced Materials Stat-Rite® S-1107 TPU Alloy
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: S-1107 is a static dissipative TPU alloy. It utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components. Features: Permanent static dissipative; Humidity insensitive; Ultra-clean: low off-gassing, low ionic contamination; Colorable; Durable: Can be used for years and years. Applications: Cleanroom Conveyor wear strips; Electronic component handling; Cleanroom Softwall Curtains; Cleanroom tubing and hose; Cleanroom Conveyor Rollers
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Clean/High Purity; Durable; ESD Protection; Good Colorability; Humidity Resistant; Low (to None) Ion Content; Low to No Outgassing; Rapid Static Decay
Uses: Conveyor Parts; Conveyor; Electrical Parts; Electrical/Electronic Applications; Hose; Rollers; Tubing
Appearance: Natural Color
Forms: Pellets
Processing Method: Extrusion; Injection Molding; Thermoforming

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ASTM D412
Tensile Strength at Break 11.5 MPa1670 psiASTM D412
Tensile Stress  4.52 MPa
@Strain 50 %
656 psi
@Strain 50 %
ASTM D412
 5.21 MPa
@Strain 100 %
755 psi
@Strain 100 %
ASTM D412
 6.43 MPa
@Strain 200 %
933 psi
@Strain 200 %
ASTM D412
Elongation at Break 700 %700 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.30e+8 ohm-cm2.30e+8 ohm-cmESD S11.12
Surface Resistance 4.80e+7 ohm4.80e+7 ohm12% RH; ESD S11.11
Static Decay 0.10 sec0.10 sec1000 V to 10 V, CPM, 50% RH
 <= 2.0 sec<= 2.0 sec5000 V to 50 V, FTMS-101C, 12% RH
 <= 2.0 sec<= 2.0 sec-5000 V to -50 V, FTMS-101C, 12% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR6019 / 268321

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.