MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Duratron™ DFU7000 PI Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: These direct-formed premium shapes offer improved thermal oxidative stability, lower moisture uptake, and better dimensional stability, on top of outstanding thermal, electrical, mechanical, and chemical resistance properties.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Water Absorption at Saturation 1.90 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105ASTM D785
Tensile Strength 95.0 MPaISO 527-1/-2 (7)
Flexural Strength 155 MPaISO 178 (12)
Compressive Yield Strength 30.0 MPa
@Strain 1.00 %
ISO 604 (10)
 50.0 MPa
@Strain 2.00 %
ISO 604 (10)
 95.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 3.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µin/in-°FASTM E-831 (TMA)
 39.0 µm/m-°C
@Temperature 23.0 - 100 °C
 41.0 µm/m-°C
@Temperature 23.0 - 150 °C
 54.0 µm/m-°C
@Temperature >=150 °C
Thermal Conductivity 0.330 W/m-K
 2.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °FContinuous Use Temperature in Air after 20000 hr
Minimum Service Temperature, Air -321 °F
 -196 °C
Glass Transition Temp, Tg 555 °FDMA- Tan d
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Acceptable
Alcohols Unacceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Unacceptable
Chlorinated Solvents Unacceptable
Continuous Sunlight Unacceptable
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Unacceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SMU762 / 323877

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.