System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Total Finathene® 3802N Natural HDPE pipe grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Pipe Grade
Material Notes:
Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe lining
Information provided provided by Total Petrochemicals.
Total Petrochemicals includes former Fina and Atofina plastics product lines.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.939
g/cc
ASTM D 792
High Load Melt Index
20
g/10 min
@Load 21.6 kg
ASTM D 1238
Mechanical Properties
Original Value
Comments
PENT
>=
5000
hour
ASTM F 1473
Hardness, Shore D
65
ASTM D 2240
Tensile Strength at Break
4000
psi
ASTM D 638 type IV
Tensile Strength, Yield
>=
2600
psi
ASTM D 638 type IV
Elongation at Break
>= 700 %
ASTM D 638 type IV
Flexural Modulus
102000
psi
ASTM D 790
Hydrostatic Design Basis
1250
psi
@Temperature 23.0 °C
ASTM D 2837
Thermal Properties
Original Value
Comments
CTE, linear
216
µm/m-°C
@Temperature 20.0 °C
ASTM D 696
Melting Point
259
°F
ASTM D3417
Vicat Softening Point
260
°F
ISO 306
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LyondellBasell Alathon® L5332CP High Density Polyethylene
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
LyondellBasell Hostalen CRP 100 RESIST CR orange High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 ORANGE High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Alathon® H5520 High Density Polyethylene
PFINAP112 / 38695
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.