MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® LXM8 Nylon 12, 8% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: VESTAMID® LXM8 is a medium-viscosity, glass fiber-reinforced and heat-stabilized polyamide 12 compound with good applicability for sport components such as shoe soles requiring very good fatigue performance and bonding ability to TPUs. Parts made of the semi-crystalline polyamide VESTAMID® LXM8 are characterized by excellent dimensional stability, constantly high impact strength, low coefficient of friction, good chemical resistance at changing ambient humidity, and excellent bonding strength to TPU. VESTAMID® LXM8 is suitable for manufacturing injection molded parts with efficient cycle times. VESTAMID® LXM8 is supplied as cylindrical granules ready for processing, in moisture barrier bags. Inside the original and undamaged packaging the product has a shelf life of at least two years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sports and Lifestyle
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Translucent
Resistance to: Heat (thermal stability), UV / light / weathering, Fatigue resistance
Electrical: Insulating
Additives: Glass fibers
Applications: General purpose
Special Characteristics: Semi-crystalline, Light-stabilized, U.V. stabilized
Color: Natural color
Additives: Antioxidant agent, Light stabilizer
Delivery form: Cylindrical pellets

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Water Absorption 0.250 %Sim to ISO 62
Moisture Absorption 0.140 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00600 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00400 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75.0ISO 7619-1
Tensile Strength at Break 55.0 MPaISO 527
Elongation at Break 16.0 %ISO 527
Tensile Modulus 2270 MPaISO 527
Flexural Modulus 1890 MPaISO 178
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 180 °CISO 11357-1/-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °C
Mold Temperature 60.0 °C
 
Descriptive Properties
Color-2.7Color a, CIE
 4Color b, CIE
 63.7Color L, CIE
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7932 / 325064

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.