MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips DRISCOPLEX® 1000 HDPE PIPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: DriscoPlex® 1000 Pipe meets or exceeds:
ASTM F714 (4” and larger)
ASTM D3035 (up to 3”)
ASTM D3350, cell classification PE445574C
PPI TR-4 designation PE4710

DriscoPlex® 1000 Pipe for: Non-Potable, Non AWWA Water Irrigation, Industrial, Agriculture
Iron Pipe Size (IPS) ¾” to 54” Solid Black 40’ and 50’ Jts 500’ coils available in sizes through 6”

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccblack; ASTM D1505
Carbon Black Loading >= 2.00 %UV Stabilizer; ASTM D3350
Melt Flow 0.0800 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 500 hourASTM F1473
Hardness, Shore D 62.0ASTM D2240
Tensile Strength, Yield >= 3500 psiASTM D638 Type IV
Elongation at Break >= 700 %2 in / min., Type IV Bar; ASTM D638
Modulus of Elasticity >= 175 ksiASTM D638
Flexural Modulus >= 120000 psi2% Secant – 16:1 span: depth. 0.5 in / min.; ASTM D790
Hydrostatic Design Basis 1000 psi
@Temperature 60.0 °C
ASTM D2837
 1600 psi
@Temperature 23.0 °C
ASTM D2837
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µin/in-°FASTM D696
Vicat Softening Point 256 °FASTM D1525
Brittleness Temperature <= -103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEVC8800 / 323303

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.