MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Selenis VENUZ XP 560 Copolyester for Cosmetics Packaging
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis Venuz XP 560 has been specifically developed for the cosmetics market where exceptional clarity is combined with high performance and easy processing, allowing efficient package designs that transmit luxury. Cosmetic parts molded from Selenis Venuz XP 560 provide good chemical resistance to most ingredients used in the industry as well as good barrier properties, helping brand owners grant product safety and preservation during storage. Packaging cost may be reduced as shelf life can be maintained even without the use of additional liners. The superior clarity of the Selenis Venuz XP 560 grade allows packaging engineers to design parts with thin walls without sacrificing transparency, maximizing consumer’s perception of a high-end product. Selenis Venuz XP 560 provides improved impact resistance, resembling the appearance of glass with the advantage of being virtually unbreakable, allowing creation of unique and personalized designs. The Selenis Venuz XP 560 copolyester is the ideal choice for injection molding. This material allows fast cycle times and may improve efficiency. Selenis Venuz XP 560 has been formulated to withstand high heat transition temperatures making it the perfect choice if the customer intends to recycle.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.790 g/cc0.0285 lb/in³
Density 1.26 g/cc0.0455 lb/in³ASTM D792 (2013)
Moisture Absorption at Equilibrium <= 0.30 %<= 0.30 %
Viscosity Test 63 - 67 cm³/g0.63 - 0.67 dl/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0<= 1.0b*; ASTM D6290
 >= 68>= 68L*; ASTM D6290
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 88.0 °C190 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 250 °C356 - 482 °F
Drying Temperature <= 70.0 °C<= 158 °Fto avoid chips sticking together in dryer hopper
 65.0 °C
@Time 21600 - 28800 sec
149 °F
@Time 6.00 - 8.00 hour
Moisture Content <= 0.0040 %<= 0.0040 %dried
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Food Approval PharmacopeiaYes
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSELE934 / 243432

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.