Hostacom TRC104NB NATRL high stiffness, high impact mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of properties and processability. It is a globally available grade typically used for automotive instrument panels and other interior applications. Availability: North America Application: Interior Automotive Applications; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Good Moldability; Good Processability; High Impact Resistance; High Stiffness; Pleasing Surface Appearance Information provided by LyondellBasell. |