MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinpolene GPP1615/2 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Availability: Africa & Middle East; Latin America; Asia Pacific; South America

Additive: Glass Fiber Reinforcement, 15% Filler by Weight

Features: Good Dimensional Stability; High Heat Resistance; Good Impact Resistance; Medium Rigidity

Uses: Automotive Applications; Housings; Pump Parts

Appearance: Colors Available

Forms: Pellets

Processing Method: Injection Molding

Information Provided by Teknor Apex

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
Linear Mold Shrinkage 0.0047 cm/cm0.0047 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0047 cm/cm0.0047 in/inASTM D955
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.0 MPa9140 psiASTM D638
Elongation at Break 11 %11 %ASTM D638
Flexural Strength 80.7 MPa11700 psiASTM D790
Flexural Modulus 4.20 GPa609 ksiASTM D790
Izod Impact, Notched 0.448 J/cm
@Temperature 22.8 °C
0.840 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
@Thickness 3.20 mm
300 °F
@Thickness 0.126 in
Unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Thermylene® P6-40FG-0684 40% Glass Fiber Reinforced, Heat and UV Stabilized Polypropylene
Asahi Kasei Thermylene® P6-30FG-0709 30% Fiber Glass Reinforced, Heat Stabilized Polypropylene
Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper Polypropylene
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene
Asahi Kasei Thermylene® P6-16FG-0801 16% Fiber Glass Reinforced, UV Stabilized Polypropylene

PTEKNP222 / 129303

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.