MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 2E98P/S2K Polyethylene Protective Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Protective Tape is a self-wound clear and printed tapes made from a co-extruded multi-polymer backing coated with a very high-tack acrylic adhesive system to help provide temporary protection of pre-tested treated truck, automotive and other hard-to-adhere carpets, fabrics interiors and carpeted door panels that require very high adhesion levels. It is printed with removal instructions. The tapes are not available in reverse wound rolls.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 3.10 MPa450 psiASTM D882
Elongation at Break 600 %600 %ASTM D882
Peel Strength 0.49303 kN/m2.8125 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypeAcrylic
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dielectric Polymers NT-590 Polyimide Film Tape
Dielectric Polymers NT-583 Linered Polyimide Film Tape
Dielectric Polymers NT-490 Polyimide Label Stock
CEN® Electronic Material CS Polyimide Tape
Aremco Pyro-Tape™ 682-ER High Temperature Tape Single layer polyimide film with silicone adhesive

PMM34301 / 169048

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.