MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool Millboard 1401 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: RCF Fiber Class. Kaowool Millboard products are processed from a slurry consisting of Kaowool ceramic fibers, fillers and binders. The fiber raw material is kaolin, a naturally occurring high-purity alumina-silica fireclay. Kaowool Millboard products are strong, thin, durable ceramic fiber based boards having a variety of high-temperature applications. Although these products were formulated and designed to replace asbestos millboard, their potential use extends into more conventional refractory fiber applications. Their use should be considered whenever there is a need for a thin, durable board with excellent insulating characteristics. Kaowool 1401 Millboard is a strong, thin, dense board product with excellent compression resistance and insulating characteristics. It is produced from Kaowool ceramic fibers, clay, inert fillers, and a small amount of both organic and inorganic binders for increased handling strength. It maintains its integrity throughout a wide temperature range and is easily fabricated and die cut.

Applications:

  • High-temperature gaskets (all grades)
  • Thermal barrier (grades 822 and 1401)
  • Backup insulation (grades 822 and 1401) Heat and flame shields (grade 1401)
  • Parting media (grade 1401)

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.560 - 0.641 g/cc
Loss On Ignition 9.0 - 11 %
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.0600 - 0.140 MPaat 5% deformation
 0.380 - 0.480 MPaat 10% deformation
 1.20 - 1.38 MPaat 15% deformation
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0800 W/m-K
@Temperature 260 °C
ASTM C201
 0.120 W/m-K
@Temperature 538 °C
ASTM C201
 0.150 W/m-K
@Temperature 816 °C
ASTM C201
 0.190 W/m-K
@Temperature 1093 °C
ASTM C201
Melting Point 1760 °C
Maximum Service Temperature, Air <= 1093 °CContinuous Use
 
Component Elements PropertiesOriginal ValueComments
Al2O3 36 %
Other 4.0 %
SiO2 60 %
 
Descriptive Properties
Classification Temperature (°C)1260
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool Millboard 822 Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Morgan Advanced Ceramics IFB Insulation Range JM™ 23-400 Thermal Ceramic
Morgan Advanced Ceramics IFB Insulation Range JM™ 23 Thermal Ceramic
Morgan Advanced Ceramics Cerox® 90V Thermal Ceramic

CMORF6070 / 202854

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.