MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

REXtac Rextac® RT 3460 Amorphous Polyalphaolefin (APAO)
Categories: Polymer; Thermoplastic; Polyalphaolefin; Polyolefin

Material Notes:
Modified Bitumen Roofing Grade.

Description: Ethylene copolymer and FDA compliant

Features: Balance high temperature resistance and low temperature flexibility

Applications: Component of modified bitumen roofing systems

Other Properties:
Ring and Ball Softening Point (ASTM E 28): 137°C.
Needle Penetration (ASTM D 1321): 25 mm.
Melt Density (190°C; Huntsman Method): 0.74 g/cc.
Flashpoint, COC (ASTM D 93): >235°C.

Information provided by Huntsman Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³ASTM D 792
Melt Density  0.740 g/cc
@Temperature 190 °C
0.0267 lb/in³
@Temperature 374 °F
Huntsman Method
 0.740 g/cc
@Temperature 190 °C
0.0267 lb/in³
@Temperature 374 °F
Huntsman Method
Viscosity  6000 cP
@Temperature 190 °C
6000 cP
@Temperature 374 °F
Melt; ASTM D-3236
 6000 cP
@Temperature 190 °C
6000 cP
@Temperature 374 °F
Melt
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -27.0 °C-16.6 °F
 -27.0 °C-16.6 °FASTM D-3418
Flash Point >= 235 °C>= 455 °FCOC; ASTM D 93
 >= 235 °C>= 455 °FCOC; ASTM D 93
Ring & Ball Softening Point 138 °C280 °FASTM E 28
 138 °C280 °FASTM E 28
 
Processing PropertiesMetricEnglishComments
Pot Life 0.500 min0.500 minOpen Time; ASTM D-4497
 0.500 min0.500 minOpen Time, Kraft/Kraft; Huntsman Method
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 YesYes
 
Descriptive Properties
Needle Penetration (mm)30ASTM D 1321

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUN26 / 47646

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.