MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Weartech International WT-694 Cobalt Hardfacing & Wear Resistant Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy

Material Notes:

Information provided by Weartech International

Key Words: PWA 694
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 47 - 54
Elongation at Yield 0.00 - 1.0 %
Charpy Impact <= 4.00 ft-lbAs Cast
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.60 µin/in-°F
Specific Heat Capacity 0.0920 BTU/lb-°F
Melting Point <= 2325 °F
Liquidus 2325 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.90 %
Chromium, Cr 28 %
Cobalt, Co 43.1 - 46.1 %
Iron, Fe <= 3.0 %
Nickel, Ni 5.0 %
Tungsten, W 19 %
Vanadium, V 1.0 %
 
Descriptive Properties
Corrosion Resistance, Hydrochloric Acid Conc. 5.65%<5 mils/yearRT
Corrosion Resistance, Nitric Acid Conc. 25-65%<5 mils/yearRT
Corrosion Resistance, Sulfuric Acid Conc. 5-10%<5 mils/yearRT
Relative Wear PerformanceCold AbrasionExcellent
 CorrosionExcellent
 ErosionExcellent
 Hot AbrasionExcellent
 ImpactNot Recommended
 Metal to MetalGood/Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PWA 1480 Nickel Alloy Composition Spec
Goodfellow Audiolloy® Iron 52/Nickel 48 Alloy
ATI Allvac® VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
ATI Allvac® Vasco® 17-4 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age
ATI Allvac® Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal

NWEART017 / 142554

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.