MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beryllium Copper, UNS C17000, TM01 Temper Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Commonly fabricated by blanking, forming and bending, turning, drilling, tapping.

Applications: bellows, bourdon tubing, diaphragms, fuse clips, fasteners, lock-washers, springs, switch parts, roll pins, valves, welding equipment.

Available as flat products, rod.

Proprietary mill heat treatment intended to produce the stated tensile properties.

Key Words: BeCu; 165 Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.26 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C >= 21>= 21
Hardness, Rockwell HR30N 42 - 4642 - 46
Hardness, Vickers 230 - 265230 - 265
Tensile Strength, Ultimate 760 - 825 MPa110000 - 120000 psi
Tensile Strength, Yield 620 - 760 MPa
@Strain 0.2 %
89900 - 110000 psi
@Strain 0.2 %
Elongation at Break 15 - 19 %15 - 19 %in 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.300.30
Fatigue Strength 230 - 260 MPa
@# of Cycles 1.00e+8
33400 - 37700 psi
@# of Cycles 1.00e+8
rotating beam
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 50.0 GPa7250 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000052 - 0.0000086 ohm-cm
@Temperature 20.0 °C
0.0000052 - 0.0000086 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.7 µm/m-°C
@Temperature 20.0 - 100 °C
9.28 µin/in-°F
@Temperature 68.0 - 212 °F
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
9.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 118 W/m-K819 BTU-in/hr-ft²-°F
 145 W/m-K
@Temperature 200 °C
1010 BTU-in/hr-ft²-°F
@Temperature 392 °F
Melting Point 865 - 980 °C1590 - 1800 °F
Solidus 865 °C1590 °F
Liquidus 980 °C1800 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 845 °C1550 °FHot-Shortness Temperature
Annealing Temperature 775 - 800 °C1430 - 1470 °F
Solution Temperature 760 - 790 °C1400 - 1450 °F
Aging Temperature 260 - 425 °C500 - 797 °F
Hot-Working Temperature 650 - 825 °C1200 - 1520 °F
Recrystallization Temperature 730 °C1350 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.6 - 1.79 %1.6 - 1.79 %
Co + Ni >= 0.20 %>= 0.20 %
Co + Ni + Fe <= 0.60 %<= 0.60 %
Copper, Cu 98.1 %98.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium Copper, UNS C17000, TM02 Temper Strip
Beryllium Copper, UNS C17000, TM00 Temper Strip
Beryllium Copper, UNS C17000, TF00 Temper Strip
Beryllium Copper, UNS C17000, TH01 Temper Strip
Beryllium Copper, UNS C17000, TH04 Temper Strip

MC17000c2 / 10730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.