MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Deranox™975 Mac-A975R Technical Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Fine grain alumina ceramic. A high quality material, widely used for electrical and mechanical components that require thick film metallizing, as well as for dynamic duties where resistance to abrasion and chemical attack are essential.

Applications:

  • Thick film metallized components, such as those with conductor and/or resistor networks, dielectric layers, solderable interfaces, etc
  • High-integrity devices for duties in the defence, aerospace, medical, laser and scientific instrument fields
  • Dynamic and static components in pumps and valves that handle corrosive or abrasive media

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.80 g/cc0.137 lb/in³fired
Porosity 0.00 %0.00 %fully dense, nominal
Grain Size 4.0 µm4.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 45 N 8585
Hardness, Vickers 1515Gpa @ Hv 0.5kg
Modulus of Elasticity 340 GPa
@Temperature 20.0 °C
49300 ksi
@Temperature 68.0 °F
Flexural Strength 350 MPa50800 psi3 point; ASTM C1161
Compressive Strength 2500 MPa363000 psi
Fracture Toughness 3.60 MPa-m½3.28 ksi-in½
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  <= 1.00e+8 ohm-cm
@Temperature 600 °C
<= 1.00e+8 ohm-cm
@Temperature 1110 °F
 <= 1.00e+12 ohm-cm
@Temperature 300 °C
<= 1.00e+12 ohm-cm
@Temperature 572 °F
 <= 1.00e+16 ohm-cm
@Temperature 20.0 °C
<= 1.00e+16 ohm-cm
@Temperature 68.0 °F
Dielectric Constant  9.5
@Frequency 9.40e+9 Hz
9.5
@Frequency 9.40e+9 Hz
 9.6
@Frequency 1e+6 Hz
9.6
@Frequency 1e+6 Hz
Dielectric Strength 20.0 kV/mm508 kV/in@ 2-3mm
Dielectric Loss Index  0.00019
@Frequency 1e+6 Hz
0.00019
@Frequency 1e+6 Hz
 0.00043
@Frequency 9.40e+9 Hz
0.00043
@Frequency 9.40e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.10 µm/m-°C
@Temperature 0.000 - 800 °C
4.50 µin/in-°F
@Temperature 32.0 - 1470 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°F
Thermal Conductivity 24.0 W/m-K
@Temperature 20.0 °C
167 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1660 °C3020 °FNo-Load
 
Component Elements PropertiesMetricEnglishComments
Al2O3 97.5 %97.5 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF8037 / 203514

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.