MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Polymer Industries Densetec PP Homopolymer Sheet
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Polymer Industries’ Densetec Homopolymer Polypropylene exhibits the properties of high corrosion resistance, high temperature resistance, and great tensile strength. It maintains its stiffness at elevated temperatures and displays resistance to organic solvents, degreasing agents, and electrolytic attack. In addition, the material is lightweight, and stain and moisture resistant. Due to its chemical resistance, Densetec Homopolymer Polypropylene is ideally suited to be used with a wide range of chemicals. Its resistance to aggressive media permits it to be used in laboratories and a large variety of industrial applications. The material resists most strong acids and bases even at relatively high temperatures and concentrations.

Information provided by Polymer Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D792
Melt Index of Compound 0.60 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 92ASTM D785
Tensile Strength, Yield 33.0 MPaASTM D638
Elongation at Yield 16 %ASTM D638
Flexural Modulus 1.552 GPaASTM D790A
Izod Impact, Notched 64.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 164 °CPrivate Lab

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
E-Polymers EFLEX® M400 PP Homopolymer

PPOLIND10 / 56986

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.