MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Capron® B85QP Nylon 6 (DAM)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Information provided by BASF Corporation.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Volatiles 0.80 %0.80 %Extractable
Water Absorption 1.6 %1.6 %24 hr.; ISO 62
 9.5 %9.5 %ISO 62
Moisture Absorption at Equilibrium 0.080 %0.080 %ASTM D570
 2.7 %2.7 %23°C/50% R.H.; ISO 62
Oxygen Transmission Rate 40.3 cc/m²/day2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm35.6 cc-mil/100 in²-24hr-atmcc/m2/day (Thickness not reported)
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm185 cc-mil/100 in²-24hr-atmcc/m2/day (Thickness not reported)
Viscosity Measurement 3.153.15Relative Viscosity (96% SAV)
 3.23.2Relative Viscosity (95% SAV)
 3.43.4Relative Viscosity (98% SAV)
 8585Formic Acid; ASTM D789
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psi2 in/min; ASTM D638
Flexural Strength 100 MPa14500 psiASTM D790
Flexural Modulus 2.62 GPa380 ksiASTM D790
Izod Impact, Notched 0.450 J/cm0.843 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM D3418
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
 
Descriptive Properties
AdditiveUnfilled
ColorNatural
Commercial Status (March 2007)Active America
Impact ModifiedNo
Primary Processing TechniqueFilm Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ALM D80-ST Nylon 11 SLS Prototyping Polymer
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Arkema Platamid® H 005 Pellets Polyamide
Arkema Platamid® H 106 Powder PA

PALBSE525 / 23176

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.