Stretchene RP1903 is a random copolymer, selected for injection stretch blow molding (ISBM) applications. The product features very good transparency and gloss. Stretchene RP1903 is typically used in packaging of detergents, cosmetics and others where ISBM bottles are used as the packaging. Applications: House wares.Information provided by LyondellBasell. |