MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Materion C110 Gold-Silver Electrical Contact Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Precious Metal; Gold Alloy; Silver Alloy

Material Notes: Has excellent conductivity, plus controllable stiffness and hardness. It is compatible with high volume stamping.

Williams Advanced Alloys is now a part of Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 15.9 g/cc0.574 lb/inĀ³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000103 ohm-cm0.0000103 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Gold, Au 75 %75 %
Silver, Ag 25 %25 %
 
Descriptive Properties
Compare To:Ney Oro 28
Tempers AvailableAR,A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free electronic Copper, UNS C10100
FloMet Fe-3% Si Soft Magnetic Alloy
Copper, UNS C12000
Eagle Brass 110 EPT COPPER, Hard
Eagle Brass 110 EPT COPPER, Annealed

NWILL95 / 19983

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.