MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® eCO E40 CC50 Nylon 12, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® eCO E40 CC50 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer. The VESTAMID® E represents thermoplastic elastomers generically characterized as polyether block copolyamides (PEBA) consisting of PA 12 and polyether segments. VESTAMID® eCO E40 CC50 is especially developed for sport shoe soles. It has good impact strength at low temperatures. eCO stands for Evoniks aim to reduce CO2 trough use of renewable or circular feedstocks via mass-balance approach. VESTAMID® eCO E40 CC50 is supplied as spherical pellets in moisture-proof packaging, ready for processing. The process temperatures should be within a range of 170°C – 210°C. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Sustainable, Industry and Engineering, Sports and Lifestyle
Sustainability: RFP (reducted foot print), eCO
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Optics: Translucent
Resistance to: Heat (thermal stability), UV / light / weathering
Additives: Unfilled
Processing: Profile extrusion
Special Characteristics: Light-stabilized, U.V. stabilized, High heat resistant
Color: Natural color
Additives: Plasticizer, Light stabilizer, Heat stabilizer

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched NB
@Temperature 23.0 °C
ISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
Tensile Impact Strength 210 kJ/m²notched, atN; ISO 8256/1
Tensile Creep Modulus, 1 hour 80.0 MPa
@Strain 0.500 %
ISO 899-1
Tensile Creep Modulus, 1000 hours 60.0 MPa
@Strain 0.500 %
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+8 ohm-cmIEC 62631-3-1
Surface Resistance 2.00e+13 ohmIEC 62631-3-2
Dielectric Constant 5.50
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 9.50
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 36.0 kV/mmAC, S20/P50; Sim. To IEC 60243-1
Dissipation Factor 0.120
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.300
@Frequency 100 Hz
IEC 62631-2-1
 
Descriptive Properties
Blue water consumption68.1 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.5 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 4.2 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 4.3 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.6 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7900 / 325032

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.