MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC 100 Thermoset Polyester, GP
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is well suited for injection, transfer or compression molding of intricate parts.

Typical applications are circuit breakers, insulators, bobbins and electrical connectors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.85 - 1.95 g/cc
Water Absorption 0.15 - 0.25 %24 hours, 23°C
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 40 - 50
Tensile Strength, Ultimate 4000 - 6000 psi
Flexural Strength 12000 - 16000 psi
Flexural Modulus 1800 - 2000 ksi
Compressive Strength 18000 - 22000 psi
Izod Impact, Notched 2.00 - 4.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 350 - 370 V/milStep by Step
 370 - 420 V/milShort Time
Arc Resistance >= 180 sec
Comparative Tracking Index >= 500 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Mold Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC 102 Glass Filled Thermoset Polyester
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman BMC 200 Thermoset Polyester, Electrical Grade
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP
Overview of materials for Polyester (Thermoset) - Rigid

PBMC000 / 27183

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.