MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Magnéli-Phase 40 vol.-% Ti4O7/60 vol.-% Ti5O9
Categories: Ceramic; Oxide; Titanium Oxide

Material Notes: Samples were hot-pressed at 1500°C and 70 MPa. Porosity is 6 Vol%. Average grain size is 5µm.

Information provided by Dr. Mathias Woydt from this reference: M. Woydt, Tribological Characteristics of Polycrystalline Titanium Dioxides with Planar Defects, Tribology Letters, 2000, Vol. 8, No. 2-3, Special Issue, "Lubricious Oxides," p. 117-130.

Key Words: titanium oxide, Ti4O7, Ti5O9, Magneli Phase
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 5.244 g/cc
Weibull Modulus 7.6
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 9630 - 10950HV 0.2
Modulus of Elasticity 221 GPa
Flexural Strength 100 MPaMedian 4 point bending strength per DIN 51110
Poissons Ratio 0.275
Shear Modulus 86.7 GPaCalculated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ti-24Al-11Nb Titanium Aluminide
Fused Quartz
Yttria Stabilized Zirconia, YSZ
Zirconium Oxide, Zirconia, ZrO2
Titanium, Ti

BTIOMG / 323

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.