MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Stat-Rite® S-102 Static Control Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Stat-Rite® S-102 is a static dissipative Polyethylene alloy. Stat-Rite® S-102 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. It is specially developed for blown film applications and is highly suitable for ESD-sensitive parts requiring a robust packaging that does not tear easily.

Features:

  • Clean, permanent, and more consistent than anti-stat
  • Provides protection for many years
  • Robust

Applications:

  • Semiconductor packaging
  • Electronic component packaging
  • Hard disk drive packaging

Available in Americas, Europe, Middle East, Africa, India and Asia

Preliminary Data Sheet

Data provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2200 psiASTM D638
Elongation at Break >= 500 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+9 ohm-cmESD S11.11
Surface Resistance 4.00e+8 ohmESD S11.11
Static Decay >= 2.0 secCharged Plate Monitor; (1000 V to 10 V)
Tribocharge 10 VNitrile Glove
 
Optical PropertiesOriginal ValueComments
Haze 37 %ASTM D1003
Transmission, Visible 84 %ASTM D1003
 
Descriptive Properties
ColorNatural, Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet)
Ineos H36G-01 Polypropylene Homopolymer
Ineos H35Z-GP Polypropylene Homopolymer
Ineos H35Z-01 Polypropylene Homopolymer

PNOVEON22a / 138280

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.