MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Morgan Advanced Ceramics TR® 2000SL Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Crystalline Silica. TR-2000 SL Block Insulation is an asbestos-free insulation, manufactured from calcium silicate and reinforced with cellulose fibers. This product is versatile and available in a wide range of sizes with either beveled or straight edges. Because of the low conductivity, the board is an economical, energy saving insulation. It exhibits minimal shrinkage at top temperature limits, and will not decompose at its maximum service temperature.

Applications:

  • Tub wall insulating material in carbon baking pits
  • Backup insulation in aluminum pot cells
  • Reheat and pusher furnaces
  • General backup insulation
  • Commercial appliances

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³ambient; ASTM C 303
Loss On Ignition 10.5 %10.5 %
Porosity 90 %90 %ASTM C493
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00107 GPa0.155 ksiambient; ASTM C 203
Compressive Strength 1.48 MPa215 psi10% deformation
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0800 W/m-K
@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 500 °F
at density 280 kg/m3; ASTM C201
 0.100 W/m-K
@Temperature 538 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 1000 °F
at density 280 kg/m3; ASTM C201
 0.140 W/m-K
@Temperature 816 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1500 °F
at density 280 kg/m3; ASTM C201
 0.160 W/m-K
@Temperature 980 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1800 °F
at density 280 kg/m3; ASTM C201
Maximum Service Temperature, Air <= 1050 °C<= 1920 °FContinuous Use
 
Component Elements PropertiesMetricEnglishComments
CaO 46 %46 %
Fe2O3 5.0 %5.0 %
SiO2 49 %49 %
 
Descriptive Properties
Classification Temperature (°C)1080
Coloroff-white
Permanent Reheat Shrinkage1[%], ASTM C356, fired 24 hours at 1038°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silres® MK Powder Silicone Resin
Thermal Ceramics TR-2000 Block Insulation
Sinotek Materials Graphite Sealing Strip Fireproofing Sealing Products
Shell Carilon® DB6G6P30 Polyketone, Lubricated, Glass-Reinforced, Injection Molding Grade
Polygon Composites Polygon Tube® Double Insulation Tubing

CMORF6100 / 202884

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.