MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Performance SiC Technical Ceramic
Categories: Ceramic

Material Notes: Ultra Pure SiC (Silicon Carbide) is made via a chemical vapour deposition (CVD) process, a method that produces very uniform material. The combination of excellent thermal, electrical and chemical properties makes CVD SiC well suited to many semiconductor, LED, and optical applications.

Applications:

  • Rapid Thermal Process (RTP) components
  • Plasma Etch components
  • Susceptors and Heating elements
  • LED wafer carriers and cover plates
  • Sputtering Targets

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 3.21 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 2800ASTM C1327
Flexural Strength 370 MPa
@Temperature 20.0 °C
ASTM C1161
 560 MPa
@Temperature 1300 °C
ASTM C1161
Fracture Toughness 2.94 MPa-m½Vickers Indentation
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 0.100 ohm-cm
@Temperature 20.0 °C
Performance ELR SiC
 <= 1.00 ohm-cm
@Temperature 20.0 °C
Performance SiC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature -40.0 - 950 °C
ASTM E228
Specific Heat Capacity 0.660 J/g-°C
Thermal Conductivity 220 W/m-K
@Temperature 20.0 °C
Performance ELR SiC; ASTM E1461
 250 W/m-K
@Temperature 20.0 °C
Performance SiC; ASTM E1461

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 304 Austenitic Stainless steel
Morgan Advanced Ceramics Performance SiC CVD SiC chemical vapor desposition Silicon Carbide
Goodfellow Titanium Diboride, TiB2
Schunk CarSIK CT Silicon Carbide
Inhance Fluoro-Seal INHANCE® Ti-9000 Titanium Carbide

CMORF8047 / 203524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.