TABOREN-PR 22 T 10-4 is a compound based on mixture of polypropylene block copolymer and polyolefin elastomer filled with 10% of talc, stabilized with a standard antioxidant additive package. It is suitable for extrusion and blow molding applications in many industrial fields with stress put on excellent processability and good surface performance.Information provided by Silon US LLC. |