MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Naval Brass, Uninhibited, Copper Alloy, UNS C46400 , H02 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: 1/2 Hard

Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Seam Weld, Capacity for Being Cold Worked

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; hot heading and upsetting; Shearing

Typical Uses: Lock Pins; Precision Shipboard Equipment; Bolts; Nuts; Rivets; Aircraft Turn buckle Barrels; Balls; Bearings; Condenser Plates; Dies, Golf Ball Production; Heat Exchanger Tube; Hub Cones; Pressure Vessels; Structural Uses; Valve Stems; Welding Rod; Decorative Fittings; Marine Hardware; Propeller Shafts; Shafting; Turn buckles; Missile Components; Baffle Plates and Flanges; Fittings

Applicable Specifications: Bar – SAE J461, SAE J463, AMS 4612, Forgings ASTM B124/B124M, AMS 4611, FEDERAL Q-B-639, ASTM B21/B21M; Bolts – ASTM F468; Forgings, Die (Hot Pressed) – ASTM B283/B283M, ASME SB283; Nuts – ASTM F467; Plate – FEDERAL QQ-B-639, ASTM B432; Plate & Sheet - for Pressure Vessels, Condensers & Heat Exchangers ASME SB171, for Pressure Vessels, Condensers & Heat Exchangers ASTM B171/B171M; Rod – AMS 4612, ASTM B21/B21M, SAE J463, SAE J461, AMS 4611, Forgings ASTM B124/B124M; Screws – ASTM F468; Shapes – Forgings ASTM B124/B124M, ASTM B21/B21M; Sheet – FEDERAL QQ-B-639; Strip – SAE J463, FEDERAL QQ-B-639, SAE J461; Studs – ASTM F468; Wire – MILITARY MIL-W-6712

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  82
@Thickness 25.4 mm
82
@Thickness 1.00 in
 85
@Thickness 6.35 mm
85
@Thickness 0.250 in
Tensile Strength  517 MPa
@Thickness 25.4 mm
75000 psi
@Thickness 1.00 in
 552 MPa
@Thickness 6.35 mm
80000 psi
@Thickness 0.250 in
Tensile Strength, Yield 393 MPa
@Thickness 6.35 mm
57000 psi
@Thickness 0.250 in
0.5% Ext
Elongation at Break  20 %
@Thickness 25.4 mm
20 %
@Thickness 1.00 in
 20 %
@Thickness 6.35 mm
20 %
@Thickness 0.250 in
Tensile Modulus 103 GPa15000 ksi
Modulus of Rigidity 38.6 GPa5600 ksi
Poissons Ratio 0.340.34Calculated
Machinability 30 %30 %
Forgeability 90 %90 %
Shear Strength  276 MPa
@Thickness 50.8 mm
40000 psi
@Thickness 2.00 in
 276 MPa
@Thickness 25.4 mm
40000 psi
@Thickness 1.00 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000610 ohm-cm0.00000610 ohm-cm28% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.2 µm/m-°C
@Temperature 20.0 - 300 °C
11.8 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 9.65 W/m-K67.0 BTU-in/hr-ft²-°F
Melting Point 888 - 899 °C1630 - 1650 °F
Solidus 888 °C1630 °F
Liquidus 899 °C1650 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 649 - 816 °C1200 - 1500 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 62 %59 - 62 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.20 %<= 0.20 %
Tin, Sn 0.50 - 1.0 %0.50 - 1.0 %
Zinc, Zn 36.8 - 40.5 %36.8 - 40.5 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC46400x8 / 292033

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.