MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Tritex TRI-F Blanket Insulation
Categories: Other Engineering Material; Composite Fibers

Material Notes: TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of varying diameters it gives TRI-F excellent acoustic properties, added rigidity and strength. This patented process also removes shot thereby making it ideal for applications that see excessive vibration. TRI-F is Biosafe, environmentally friendly and manufactured from 100% recycled raw materials. TRI-F is also classified by IARC as Group 3 and is not classifiable as carcinogenic to humans.

Information provided by TRITEX

Key Words: Insulation
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.75 - 2.90 g/cc0.0994 - 0.105 lb/in³
Loss On Ignition <= 0.50 %<= 0.50 %
Filament Diameter 6.0 µm6.0 µmAverage
Absorption Coefficient  0.040
@Frequency 125 Hz
0.040
@Frequency 125 Hz
Sound
 0.12
@Frequency 250 Hz
0.12
@Frequency 250 Hz
Sound
 0.31
@Frequency 500 Hz
0.31
@Frequency 500 Hz
Sound
 0.64
@Frequency 1000 Hz
0.64
@Frequency 1000 Hz
Sound
 0.78
@Frequency 2000 Hz
0.78
@Frequency 2000 Hz
Sound
 0.87
@Frequency 4000 Hz
0.87
@Frequency 4000 Hz
Sound
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 552 MPa80000 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0807 W/m-K
@Temperature 371 °C
0.560 BTU-in/hr-ft²-°F
@Temperature 700 °F
 0.0994 W/m-K
@Temperature 482 °C
0.690 BTU-in/hr-ft²-°F
@Temperature 900 °F
 0.160 W/m-K
@Temperature 649 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 0.200 W/m-K
@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1500 °F
Melting Point >= 1100 °C>= 2010 °FFiber
Maximum Service Temperature, Air 815 °C1500 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 14 %14 %Primary Fiber
CaO 15 %15 %Primary Fiber
FeO 0.10 %0.10 %Primary Fiber
MgO 7.5 %7.5 %Primary Fiber
MnO 10 %10 %Primary Fiber
Other 3.4 %3.4 %Primary Fiber
SiO2 42 %42 %Primary Fiber
 
Descriptive Properties
Average Fiber Length (mm)4
Colorwhite/beige
Moisture ResistantYes
Surface TreatmentNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRIT002 / 90246

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.