MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Monprene® CP-18926 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-18926 is a general purpose thermoplastic elastomer designed for consumer product applications requiring a soft, rubber-like feel. Monprene CP-18926 is a low hardness that exhibits excellent moldability, suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Flexibility; Good Moldability; High Flow; Light Stabilized; Low Density; Low Specific Gravity; Low Hardness; Lubricated; Slip; Without Fillers

Uses: Consumer Applications; Gaskets; Handles; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  26
@Time 5.00 sec
26
@Time 0.00139 hour
Injection Molded; ASTM D2240
 28
@Time 1.00 sec
28
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 6.40 MPa928 psi20 in/min, Flow; ASTM D412
 6.73 MPa976 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  0.614 MPa
@Strain 100 %
89.0 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 0.634 MPa
@Strain 100 %
92.0 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 1.21 MPa
@Strain 300 %
175 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 1.23 MPa
@Strain 300 %
179 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 580 %580 %20 in/min, Across Flow; ASTM D412
 630 %630 %20 in/min, Flow; ASTM D412
Tear Strength 15.1 kN/m86.0 pli20 in/min, Across Flow; ASTM D624
 16.0 kN/m91.0 pli20 in/min, Flow; ASTM D624
Compression Set 20 %
@Temperature 22.8 °C,
Time 79200 sec
20 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 171 - 193 °C340 - 380 °FMelt, Injection
Rear Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Middle Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Front Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Nozzle Temperature 171 - 193 °C340 - 380 °FInjection
Zone 1 160 - 182 °C320 - 360 °FExtrusion
Zone 2 160 - 182 °C320 - 360 °FExtrusion
Zone 3 160 - 182 °C320 - 360 °FExtrusion
Zone 4 160 - 182 °C320 - 360 °FExtrusion
Zone 5 160 - 182 °C320 - 360 °FExtrusion
Die Temperature 160 - 182 °C320 - 360 °FExtrusion
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)

PTEKNQ0800 / 237291

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.