MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Asahi Kasei DELPET™ SRB100 Acrylic (PMMA), High Impact
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: DELPET™ has excellent transparency, surface hardness and weatherability. Main applications of DELPET™ are outer/inner parts for automobile, optical goods, industrial and general parts/goods.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³1183
Water Absorption 0.30 %
@Temperature 23.0 °C
0.30 %
@Temperature 73.4 °F
ISO 62 Method 1
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inAsahiKasei Method
Melt Flow 4.6 g/10 min
@Load 3.80 kg,
Temperature 230 °C
4.6 g/10 min
@Load 8.38 lb,
Temperature 446 °F
1133, cond 13
Spiral Flow 36.0 cm
@Thickness 2.00 mm,
Pressure 75.0 MPa
14.2 in
@Thickness 0.0787 in,
Pressure 10900 psi
cylinder temp 250°C, mold temp 60°C; AsahiKasei Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 82822039-2
Tensile Strength at Break 67.0 MPa9720 psi527-2/1A/5
Elongation at Break 24 %24 %527-2/1A/5
Tensile Modulus 2.90 GPa421 ksi527-2/1A/1
Flexural Strength 113 MPa16400 psi178
Flexural Modulus 2.90 GPa421 ksi178
Charpy Impact Unnotched 2.30 J/cm²10.9 ft-lb/in²179/1eU
Charpy Impact, Notched 0.120 J/cm²0.571 ft-lb/in²179/1eA
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 97.0 °C207 °FDeflection Temperature, load not reported; ISO 75-1
Vicat Softening Point 104 °C219 °F306 B50
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49489
UV Transmittance 92 %92 %13468-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei DELPET™ 720V Acrylic (PMMA), Standard Grade
Asahi Kasei DELPET™ SRJ259 Acrylic (PMMA), High Impact
LG Chemical HF-380 ABS, High Flow, High Impact
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Asahi Kasei DELPET™ SRE255 Acrylic (PMMA), High Impact

PASAHI8033 / 221060

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.