MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Leaded Tin Bronze, UNS C92300, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand.

Applications: Valves, pipe fittings, and high-pressure steam castings. Superior machinability to C90300.

Classified under: Leaded tin bronzes. ASTM B584; formerly ASTM B143-2B

Data typical for sand-cast test bars. Alloy does not respond to heat treating

Key Words: Leaded tin bronze, ASTM B584; ASTM B143-2B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 70
Tensile Strength, Ultimate 275 MPa
Tensile Strength, Yield 138 MPa
@Strain 0.5 %
Elongation at Break 25 %in 50 mm
Modulus of Elasticity 97.0 GPa
Compressive Strength 69.0 MPaat permanent set of 0.1%
 240 MPaat permanent set of 10%
Machinability 42 %UNS C36000 (free-cutting brass) = 100%
Izod Impact 18.3 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000014367 ohm-cm
@Temperature 20.0 °C
12% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 177 °C
Specific Heat Capacity 0.376 J/g-°C
Thermal Conductivity 75.0 W/m-K
Melting Point 855 - 1000 °C
Solidus 855 °C
Liquidus 1000 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 260 °CStress-Relieving Temperature
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.25 %
Copper, Cu 85 - 89 %
Iron, Fe <= 0.25 %
Lead, Pb <= 1.0 %
Nickel, Ni <= 1.0 %
Phosphorus, P <= 0.050 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.050 %
Tin, Sn 7.0 - 9.0 %
Zinc, Zn 2.5 - 5.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tin Bronze, UNS C90500, Copper Casting Alloy
Leaded Tin Bronze, UNS C92700, Copper Casting Alloy
Leaded Tin Bronze, UNS C92600, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Tin Bronze UNS C90300, Copper Casting Alloy

MC92300b1 / 11938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.