Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes:- High flexibility
- Low plasticizer migration (low blooming)
- Very good chemical resistance
- Good light and heat stability
- Good dimensional stability
Application examples: Flexible hoses and profiles, pneumatic tubes.Information provided by EMS Grivory. |