System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Epoxy
;
Epoxy Adhesive
Material Notes:
Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Brookfield Viscosity
35000
-
75000
cP
35000
-
75000
cP
Base, RVF #7 spindle, 20 rpm @ 27°C
45000
-
65000
cP
45000
-
65000
cP
Accelerator, RVF #7 spindle, 20 rpm @ 27°C
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
70
70
ASTM D2240
Tensile Strength at Break
22.8
MPa
3310
psi
ASTM D882
Elongation at Break
125 %
125 %
ASTM D882
Shear Strength
0.414
MPa
60.0
psi
Overlap, Polypropylene
1.72
MPa
250
psi
Overlap, +3M Primer 3901
2.76
MPa
400
psi
Overlap, Glass, Borosilicate
3.59
MPa
520
psi
Overlap, ABS
3.79
MPa
550
psi
Overlap, Acrylic
5.17
MPa
750
psi
Overlap, PVC
6.07
MPa
880
psi
Overlap, Polycarbonate
6.21
MPa
900
psi
Overlap, Wood, Fir
12.4
MPa
1800
psi
Overlap, Fiberglass
13.1
MPa
1900
psi
Overlap, Cold Rolled Steel
15.2
MPa
2200
psi
Overlap, Sanded Aluminum
23.4
MPa
3400
psi
Overlap, Etched Aluminum
2.76
MPa
@Temperature 82.0 °C
400
psi
@Temperature 180 °F
Overlap
3.10
MPa
@Temperature 66.0 °C
450
psi
@Temperature 151 °F
Overlap
4.83
MPa
@Temperature 49.0 °C
700
psi
@Temperature 120 °F
Overlap
23.4
MPa
@Temperature -55.0 °C
3400
psi
@Temperature -67.0 °F
Overlap
29.6
MPa
@Temperature 21.0 °C
4300
psi
@Temperature 69.8 °F
Overlap
Peel Strength
0.351
kN/m
2.00
pli
180°
0.526
kN/m
3.00
pli
180°
0.526
kN/m
3.00
pli
180°
3.16
kN/m
18.0
pli
180°
6.14
kN/m
35.0
pli
180°
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+11
ohm-cm
1.00e+11
ohm-cm
ASTM D257
Dielectric Constant
6.3
@Frequency 1000 Hz
6.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength
26.8
kV/mm
@Thickness 0.762 mm
680
kV/in
@Thickness 0.0300 in
ASTM D149
Thermal Properties
Metric
English
Comments
CTE, linear
98.0
µm/m-°C
@Temperature 5.00 - 20.0 °C
54.4
µin/in-°F
@Temperature 41.0 - 68.0 °F
Below Tg
187
µm/m-°C
@Temperature 65.0 - 140 °C
104
µin/in-°F
@Temperature 149 - 284 °F
Above Tg
Thermal Conductivity
0.151
W/m-K
@Thickness 6.35 mm,
Temperature 44.3 °C
1.05
BTU-in/hr-ft²-°F
@Thickness 0.250 in,
Temperature 112 °F
Glass Transition Temp, Tg
12.0
°C
53.6
°F
Onset
23.0
°C
73.4
°F
Mid-Point
Processing Properties
Metric
English
Comments
Cure Time
150
min
2.50
hour
Time to Handling Strength
420
min
7.00
hour
Full
Tack-Free Time
120
min
2.00
hour
Descriptive Properties
Appearance
Amber
Accelerator
Gray
Base
Gray
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M Scotch-Weld™ DP620NS Structural Adhesive
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M 760 Hybrid Adhesive Sealant
PMM34622 / 169369
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.