MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Arcol® F-1080 Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Arcol F-1080 polyol is a 3,000-molecular-weight triol.

Properties / Applications: Arcol F-1080 polyol is designed for the production of one-shot flexible urethane slabstock foams. The full range of flexible foams from extra soft to extra firm, with varying densities, can be made with Arcol F-1080 polyol. Compared to conventional 3,000-molecular-weight slabstock polyols, Arcol F-1080 has the advantage of lower tin catalyst requirements and wider tin processing latitude. Good foam physical properties are obtained over the entire range. As with any product, use of Arcol F-1080 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Bulk Density 1.03 g/cc0.0372 lb/in³
Viscosity 480 cP480 cP
 50 cP
@Temperature 85.0 °C
50 cP
@Temperature 185 °F
 100 cP
@Temperature 35.0 °C
100 cP
@Temperature 95.0 °F
 300 cP
@Temperature 35.0 °C
300 cP
@Temperature 95.0 °F
Storage Temperature 15.0 - 60.0 °C59.0 - 140 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.020<= 0.020[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 195 °C383 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50 Pt-Co
Hydroxyl number54.7-57.5 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Arcol® F-3040 Polyol
Covestro Arcol® F-3022 Polyol
Covestro Arcol® F-1522 Polyether Polyol
Covestro Arcol® E-919 Polyether Polyol
Covestro Arcol® E-434 Polyether Polyol

PCOVEST0021 / 201804

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.