MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adstif Metocene HM 2015 Metallocene-catalyzed homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability. Metocene HM2015 is a metallocene-catalyzed homopolymer for compounding and injection molding with very high melt flow rate. It contains a basic stabilization package. Metocene HM2015 has an excellent stiffness, outstanding organoleptic properties and a low warpage. Applications: Exterior Automotive Applications, Interior Automotive Applications, Opaque Containers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D 792
Melt Flow 140 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength, Yield 34.0 MPaASTM D 638
Elongation at Yield 7.0 %ASTM D 638
Flexural Modulus 1350 MPaASTM D 790
Izod Impact, Notched 20.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
 
Descriptive Properties
Processing MethodCompounding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Starflex® GM1835CAX01 Metallocene Linear Low Density Polyethylene, Film Extrusion Grade
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade)
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin
ExxonMobil ACHIEVE 3825 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications

PEQT7015 / 218654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.